T O P
manythanksmmk

If you’re printing a lot at high temps, consider purchasing an mk8 heat break from slice engineering. The ptfe tubes degrade and emit toxic fumes in temps greater than 245C or so. The mk8 heat break allows me to max out temps on snapmaker without difficulty. Hope this helps!


R2sFoot

Yeah I’m really just printing in PETG for a couple of projects. Was experimenting at 250 for awhile but based on results am going back down to 235ish. Somehow i can’t find the length of this very replaceable item on the internet. Haha